DickH
12-10-2002, 07:51 PM
I need cam locks (part #W-10070-3) and plug (part #490797) for a Hobart G-225-K welder. Any suggestions where I might find them? Thanks
Hobart Expert Dave
12-11-2002, 08:22 PM
You are not going to find the exact replacment for this any longer. What I would sugjest is call Miller Light Industrial and ask for the plug kit and recepticals fthat were used on the old Thunderbolt welders. They will fit onto this welder with out much trouble. Try them at 1-800-332-3281.
Thanks
Dave Evans