What process and procedure do railroads use to weld rails together? Thanks, Ron

Rod MI
12-07-2002, 01:15 AM
Hi there are many ways of welding them thermite welding is one

http://www.trackwelding.com/thermite.jpg

http://www.rtands.com/sep99/rail_welding.html

http://www.railroadextra.com/tkweld.Html

Rocky D
12-08-2002, 08:05 AM
Here's another one.