View Full Version : problems with m.i.g. welding mild steel and guided bend test.

02-16-2004, 03:09 PM
the two root bends are fine but the face bend always breaks away on one side,any ideas?

02-16-2004, 04:29 PM
The most common cause of this problem I have seen are the welds are brought just up to the edge of the plate and not rolled over the edge. Scott