chriswelds
12-01-2002, 03:14 PM
i own a hobart 135. my question is was should my regulator be set at for argon mix. thanks
Should be a decal with gas flow rates cfh (cubic feet per hour) on the inside of the cover on the wire feed side.
Bob
Rocky D
12-02-2002, 02:08 AM
40 CFH should give you good results...it's not that critical...if you are icing your regulator just turn it down some.