11-20-2002, 07:17 AM
Will the PC-300 work with a Syncrowave 300? I know that the Syncrowave has a 5 pin connector, but there is an adaptor to go from 14 pin to 5 pin. Will these work together? Does it work in AC mode also?
Hobart Expert Rock
11-24-2002, 11:39 PM
BUGEYEDVALIANT.......WELL SIR RIGHT OUT OF THE BOOK IT SAYS THE PC-300 CAN BE USED WITH AC OR DC WELDING POWER SOURCES WITH, OR WITHOUT, BUILT IN HIGH FREQUENCY OR WITH EXTERNAL HIGH REQUENCY UNITS FOR EXAMPLE HF-251-D1.. SO IF I'M READING THIS CORRECTLY YES IT CAN BE USED WITH THE SYNCROWAVE.............................ROCK