hi guys just a few pics of some tig 6" carbon sch 40 .the set uo is 4mm gap and fether edge prep,125-130 amp root...175amp fill and cap
urch55
02-16-2011, 09:09 PM
Looks good you're hired.:)
TozziWelding
02-19-2011, 09:02 AM
Nice work, hop a boat and we have plenty of work for you:D
fillncap
02-19-2011, 02:34 PM
cheers guys,if i had the money id be very tempted to jump a boat,work over my way is very quiet at the moment,been like this for couple of years realy..
jay
SidecarFlip
02-19-2011, 05:12 PM
You gotta love weld candy.....:D
hockeyguynick
09-27-2011, 07:52 PM
Looks very good, I'm not used to seeing those big weaves. Wish I could do it, my job requires us to show 2 beads on the reinforcement