View Full Version : Anyone ever heard of a L-tec 250 stk

11-13-2010, 01:59 PM
I have heard of and used an L-tec 250HF machine but I have run accross an L-tec 250 stk. It is labeled square wave but I can not tell if it is still HF (i doubt it). Just never heard of the stk version


12-08-2010, 11:53 PM
If it's a squarewave machine it would have to be HF. It's my understanding that you need the HF to maintain the arc in AC.