dsweld
06-16-2008, 07:20 PM
today i found out that i passed the pipe test with flying colors.asme 6g ,2" sched 80 certified.i saw the x-ray of my test no inclusions or porosity.the inspector gave me an A- for an overall grade.just a verbil grade nothing on the cert paper, just passed.the thing that hurt me was a not so tight cap.it looked pretty good but not perfect.the suckback problem i originally had was hard to correct but i did it.now i have to take a 6" sched 80 carbon, 6g, pipe test,5p root 7018 cap.never done this one either but i'm not afraid of it.thanks for all your help guys i'll keep in touch....