PDA

View Full Version : Need to rig a turntable to cut doughnuts...



243
04-17-2008, 08:21 AM
...I need a fixture to hold my O/A torch and something to hold 1/4" plate so that I can rotate the steel to cut 6"-8" diameter circles. Has anyone already done this and if so, do you have any pictures of how you did it?

whateg0
04-17-2008, 08:48 AM
Actually, the normal thing to do is to use a circle cutting fixture for the torch. It allows the torch to rotate around a point.

Here's a circle cutter on Miller's website. This one is for a plasma cutter, but the concept is the same.
http://www.millerwelds.com/education/articles/images/Fig5CircleLOW_000.jpg

I made my own, but I don't seem to have any pics handy here at work.

Dave

vicegrip
04-17-2008, 08:53 AM
Actually, the normal thing to do is to use a circle cutting fixture for the torch. It allows the torch to rotate around a point.

Here's a circle cutter on Miller's website. This one is for a plasma cutter, but the concept is the same.

I made my own, but I don't seem to have any pics handy here at work.

Dave

Dave.
Insert "the Useual thing" to do.
Some times the reverse becomes the norm.;)

vg

tnmike
04-17-2008, 08:59 AM
Handy Auto was the gas variety. Slick little rig..they still make em Im about positive