the boy and i are restoreing a old probe generation 1 what is a good product to clean up them old rim [aluminum] .

Hotfoot
03-07-2008, 09:26 PM
???Are you asking how to clean up corroded aluminum rims on a Ford Probe?????:confused:

thebighammer1
03-08-2008, 03:59 PM
all i got was a left and right scroll bar

Mechtech
03-10-2008, 09:23 AM
Check here for a better answer.

http://www.autorestorer.com/index.html

But Depending on the amount of corrosion any metal polish and some elbow grease should work.