...done in time for Christmas, but barely.

Bent from 1/4 in., 3/16ths and 1/8th in. hot rolled. Bent over my knee or over a piece of railroad iron using a ball pein hammer.

Bob the Welder
01-22-2008, 12:49 PM
That's great, a really fantastic job. I'm sure it will be greatly appreciated.

lcats
01-22-2008, 01:07 PM
Nice work, great craftsmanship. If you made the gal and guy 25-30 pounds heavier, you could put big towels and more stuff.

usmcpop
01-22-2008, 01:46 PM
Hope your knee is OK. Every time I try to bend something over my thumb using a ball pein hammer, it hurts for quite awhile. :D