I am looking for an operating manual--appreciate any help you can give.

Dayton 3Z913F
Serial # HO 42530
dated 6/18/96
Model # 111 051-009

HEAVY CHEVY
01-05-2008, 03:13 PM
I Have An Older Dayton Spot Welder And It Was Made By Miller,i Had To Replace The Switch,called Miller,they Had One In Stock And Sent It To Me.

Rocky D
01-05-2008, 03:31 PM
I googled it for awhile, and came up with...it's a Grainger product, but made by Chiry in China...don't know if this helps or hinders...:confused:

cope
01-05-2008, 07:34 PM
Century made some Dayton and Craftsman welders, as well as those sold by Matco, Mac and Snap-On.

gatkeper1
01-06-2008, 03:02 AM
3Z913 Dayton was also sold as Sears 20102, Montgomery Wards 58049 and SD Lee 100 Amp Mig