Finally broke down and purchased a Bluestar 185. Still sitting in the back of the PU as I figure out how to unload it...

Has anyone run a spoolgun off a Bluestar? Either a Miller one, or maybe a Ready Welder. According to RW, their spoolgun will
work off a CC or CV DC source. I am thinking about this setup for
aluminum welding as much as for steel.

Any input much appreciated.

twhite
04-12-2008, 04:26 PM
I've got a ready welder and have use it with a bobcat 225 and a old miller dailarc and it worked out pretty good on both for field & shop use.I have't welded alluminum with it yet, but as long as you're used to welded alluminum using the mig process you should be okay.