View Full Version : SHield gas for mild steel?



Jason280
10-13-2007, 05:21 PM
I ordered a Weldcraft air-cooled TIG torch for my Lincoln this week, and the only thing left to get is a bottle of shield gas. Can I use a standard 75/25 argon/CO2 mix TIG welding on mild steel, or will I need something else?

hankj
10-13-2007, 05:23 PM
100% argon.