View Full Version : HH187, MM180, or lincoln PM180/SP175
pucancakes
09-29-2007, 12:40 AM
differences between them? one better than the other?
whats the thickest a 140 can weld in a single pass?
Sully2
09-29-2007, 07:57 AM
whats the thickest a 140 can weld in a single pass?
3/16ths if its a prep'd weld.
Sberry
09-29-2007, 08:55 AM
Right now the common consensus is that the HH187 or the HH210 is in the lead. As for the 140 if you are already willing to consider a larger machine dont look back. The 187 class is twice the welder as the smaller one.