the Handler® 125 operates off 115-volt household current. Comes ready to weld without shielding gas using .030-.035 in (0.8-0.9 mm) flux cored wire. For greater versatility, upgrade the Handler 125 with the optional MIG conversion kit for welding with .023-.030 in (0.6-0.8 mm) solid wire and gas shielding. Use C-25 gas (75% argon/25% CO2) on 24 gauge - 1/8 in steel for a cleaner weld with less spatter. Use Tri-Mix gas and stainless wire for welding on 16-12 gauge stainless steel.
| Comes complete with: |
|
||||
|---|---|---|---|---|---|
| Power: |
|
||||
| Processes: |
|
||||
| Material Thickness: | Welds 20 gauge up to 3/16 inch | ||||
| Skill Level: | Low | ||||
| Applications: |
|
| #770187 |
Running Gear/Cylinder RackHolds large or small cylinder (not included) with tray underneath for cables |
|---|---|
| #194776 |
Small Running Gear/Cylinder RackFor gas cylinders no larger than 7in/178mm diameter (max weight 75lbs/34kg) |
| #225397 |
H-9B Replacement Welding Gun For .023 - .035 in. (0.6 - 0.9 mm) diameter wire. Includes 8 ft. cable. |
| #195216 |
Hub Kit Add to accommodate 8 in (51 mm) spools. |
| #195186 |
Protective CoverWeatherproof nylon resists stains and mildew, and protects the finish of your welder. |
|
Welding Wire Thickness Charts View Chart |
|
|
MIG Consumables for Handler 125 View Chart |
| Stock Numbers | #500495 115 VAC, 60 Hz | ||
|---|---|---|---|
| Rated Output at 20% Duty Cycle | 85 A at 17.5 VDC | ||
| 60 A at 20 VDC (CSA Rating) | |||
| Current Range | 30 - 125 A | ||
| Max. Open-Circuit Voltage | 26 V | ||
| Wire Feed Speed Range |
0 - 415 IPM 0 - 500 IPM at no load |
||
| Amps Input at Rated Load, 60 Hz | 115 V | 20 | 15 CSA Rating |
| kVA | 2.9 | 2.2 CSA Rating | |
| kW | 2.5 | 1.77 CSA Rating | |
| Dimensions | H: 16 7/8 in (429 mm) W: 9 7/8 in (251 mm) D: 12 1/8 in (308 mm) |
||
| Net Weight | 50 lb (22.7 kg) | ||
| Processes Recommended |
Steel | Stainless Steel |
Aluminum | Cast Iron | Copper | Brass | Titanium | Magnesium Alloys |
|---|---|---|---|---|---|---|---|---|
| MIG [GMAW] | X* | X* | ||||||
| Flux Cored [FCAW] | X | X* | ||||||