The Stickmate LX 300 AC/200 DC is the premium 300 amp stick welder available in the USA with enough power to get through the big jobs. Assembled in Troy, Ohio, this 300 amp stick welder offers both AC and DC output, enabling you to use specialty electrodes for a variety of metals including mild steel, cast iron, aluminum and more. Simple precision control allows you to fine-tune the arc while clearly showing the amperage you plan to weld at.
| Comes complete with: |
|
||
|---|---|---|---|
| Power: |
|
||
| Processes: |
|
||
| Skill Level: | Moderate | ||
| Applications: |
|
The power-packed Hobart Stickmate 300 AC/DC stick welder… because too much power is never enough.
| #043927 |
Running GearMounts easily to unit and provides convenient portability. Includes two wheels, two feet, and a handle. |
|---|---|
|
Stick Electrodes View Electrode Chart |
| Stock Number | #500560 Standard |
|---|---|
| Rated Output at 32.5 VAC |
AC: 250 A at 20% Duty Cycle, 60 Hz 250 A at 15% Duty Cycle, 50 Hz |
| Rated Output at 25 VDC |
DC: 175 A at 20% Duty Cycle, 60 Hz 175 A at 15% Duty Cycle, 50 Hz |
| Max. Open-Circuit Voltage AC/DC | 80 V |
| Welding Amperage Ranges |
AC High: 180 - 300 A Low: 40 - 200 A |
| DC: 30 - 200 A | |
| Amps Input at Rated Output, 60 Hz | 230 V: 72 AC, 65 DC |
| Dimensions | H: 18 3/4 in (476 mm) W: 12 3/4 in (323 mm) D: 17 1/2 in (445 mm) |
| Net Weight | 132 lb (60 kg) |
| Processes Recommended |
Steel | Stainless Steel |
Aluminum | Cast Iron | Copper | Brass | Titanium | Magnesium Alloys |
|---|---|---|---|---|---|---|---|---|
| Stick | X | X | X |