These lightweight, air-cooled units are portable, easy to operate, and provide a quick and effective means for spot welding mild, galvanized or stainless materials. These units are an excellent choice for maintenance work, and for spot welding applications that require portability and lower amperage welding.

Comes complete with:
  • Power Cord with Plug
  • Standard 6 in (152 mm) Tongs
  • Standard Tips
Power:
  • 1 Phase
Processes:
SpotResistance Spot Welding
Material Thickness: HSW-15 welds up to 1/8 inch total thickness
HSW-25 welds up to 3/16 inch total thickness
Skill Level: Low
Applications:
  • Maintenance
  • Sheet Metal Work
  • Auto Body
Tip Notes
  • One set of tips is supplied with each set of tongs
  • Maximum welding capabilities are obtained with minimum tong length
  • Tips are made of RWMA Class 2 alloy
  • Accommodates a wide variety of tongs and tips
  • Hand lever locks tongs firmly on material, ensures positive, accurate fit-up
  • Quick and easy adjustment for material thickness
  • Reversible for left- or right-hand operation
  • Includes 6 in (152.4 mm) tongs and tips

#041081
#041082
Spot Weld Timer
HSW-15
HSW-25

For air-cooled spot welders. Provides 0 - 5 second mechanical weld timer. The Timer Panel can be mounted on the SWP-2 pedestal, or any other convenient location.
  Tongs and Tips
View Chart

Standard tongs and tips are available from Hobart retailers. Other optional tongs and tips are available from welding distributors. See a Hobart retailer for product availability.
Stock Number #500440 HSW-15
Input 50/60 Hz 110 VAC, 30 A
Work Capacity* 1/8 in. (3.2 mm)
Rated Output at 50% Duty Cycle 1.5 kVA
Rated Output** 6 in / 12 in / 18 in 5550 A / 4500 A / 3600 A
Max Open-Circuit Voltage 1.6
Dimensions H: 6 in (152 mm)
W: 3 1/4 in (83 mm)
D: 13 in (330 mm)
Net Weight 22 lb (10 kg)
 
Stock Number #500442 HSW-25
Input 50/60 Hz 220 VAC, 30 A
Work Capacity* 3/16 in. (4.7 mm)
Rated Output at 50% Duty Cycle 2.5 kVA
Rated Output** 6 in / 12 in / 18 in 6750 A / 5800 A / 4850 A
Max Open-Circuit Voltage 2.5
Dimensions H: 6 in (152 mm)
W: 3 1/4 in (83 mm)
D: 16 in (406 mm)
Net Weight 30 lb (14 kg)
* Combined thickness uncoated mild steel using 6 in (152 mm) tongs
** With standard tongs
6 in = 152 mm • 12 in = 305 mm • 18 in = 457 mm

 

Processes
Recommended
Steel Stainless
Steel
Aluminum Cast Iron Copper Brass Titanium Magnesium
Alloys
Resistance Spot X X