the Handler® 187 delivers 185 amps of wire (MIG) welding power in a small package. It capable of welding 24 gauge to 5/16 steel and handles a variety of materials including mild steel, stainless steel, and aluminum. Operating on 230 volt input power, this wire welder includes everything you need to weld with flux cored self-shielding wire (great for outdoor welding projects) or solid wire (just add preferred wire and shielding gas).
| Comes complete with: |
|
||||
|---|---|---|---|---|---|
| Power: |
|
||||
| Processes: |
|
||||
| Material Thickness: | Welds 24 gauge up to 5/16 inch | ||||
| Skill Level: | Low | ||||
| Applications: |
|
| #770187 |
Running Gear/Cylinder RackHolds large or small cylinder (not included) with tray underneath for cables. |
|---|---|
| #194776 |
Small Running Gear/Cylinder RackFor gas cylinders no larger than 7in/178mm diameter (max weight 75lbs/34kg) |
| #300143 |
Spool Gun 3035-20Comes with 20 ft (6.1 m) cable and gas hose. For .030 - .035 (0.8 - 0.9 mm) aluminum, steel and stainless steel. |
| #043856 |
Spool Gun Control SGA-100 Required to connect spool gun to the Handler® 135, 140, 175, 180, or 187. Allows you to connect a spool gun to virtually any similar MIG welder — Hobart or other brands. |
| #195957 |
H-10 Replacement MIG Gun For .030 - .035 in. (0.8 - 0.9 mm) wire. Includes 10 ft. cable. |
| #193973 | M-10 Convenience Kit |
| #195186 |
Protective CoverWeatherproof nylon resists stains and mildew, and protects the finish of your welder. |
|
Welding Wire Thickness Charts View Chart |
|
|
MIG Consumables for Handler 140 & 187 View Chart |
| Stock Numbers |
#500525 230 VAC, 60 Hz #500527 230 VAC, 60 Hz with Small Running Gear/Cylinder Rack |
|
|---|---|---|
| Rated Output at 30% Duty Cycle | 130 A at 21.5 VDC | |
| Current Range | 25 - 185 A | |
| Max. Open-Circuit Voltage | 30 V | |
| Wire Feed Speed Range | 40 - 700 IPM 50 - 740 IPM at no load |
|
| Amps Input at Rated Load, 50/60 Hz | 230 V | 20.5 |
| kVA | 4.7 | |
| kW | 3.88 | |
| Dimensions | H: 12-3/8 in (315 mm) W: 10-5/8 in (270 mm) D: 19-1/2 in (495 mm) |
|
| Net Weight | 68 lb (31 kg) | |
The Handler® 187 features a 7-position voltage switch, three more positions than the original Handler® 180. These added settings create a welding arc that more perfectly matches metal thickness and wire diameter than any competitor in its class. The improved arc means less spatter, professional bead appearance, excellent penetration, and minimal post-weld cleanup.
Convenience features include internal storage area for spare tips and a "no tools" quick-change drive roll system with dual grooves to make changing wire diameter easy. A self-resetting thermal overload system protects the Handler® 187 in the toughest applications.
| Processes Recommended |
Steel | Stainless Steel |
Aluminum | Cast Iron | Copper | Brass | Titanium | Magnesium Alloys |
|---|---|---|---|---|---|---|---|---|
| MIG [GMAW] | X | X | X | |||||
| Flux Cored [FCAW] | X | X | ||||||